Loading

Report as inappropriate

I used this with support, i turn it around so it lays on the bottom side. PLA white and it looks very good with layer hight 0.2
But the baseplate with this small shaft are not good. Here i used PETG. Don´t know here is a problem of this PETG or my settings.
Now i draw my own baseplate with a thicker shaft...hope this will work.