Slic3r Settings I used:

; generated by Slic3r 0.7.1 on 2012-04-14 at 17:41:33

; layer_height = .25
; perimeters = 1
; solid_layers = 4
; fill_density = .90
; nozzle_diameter = 0.5
; filament_diameter = 1.70
; extrusion_multiplier = 1.0
; perimeter_speed = 50
; infill_speed = 40
; travel_speed = 130
; extrusion_width_rat
io = 1.45
; scale = 1
; single wall width = 0.36mm

191C Hot End (216C For First Layer), 75C Bed